Yan-hua Liu, Chao Yang, Pei-you Li, and Shi-qi Li, A new process of extracting vanadium from stone coal, Int. J. Miner. Metall. Mater., 17(2010), No. 4, pp. 381-388. https://doi.org/10.1007/s12613-010-0330-8
Cite this article as:
Yan-hua Liu, Chao Yang, Pei-you Li, and Shi-qi Li, A new process of extracting vanadium from stone coal, Int. J. Miner. Metall. Mater., 17(2010), No. 4, pp. 381-388. https://doi.org/10.1007/s12613-010-0330-8
引用本文 PDF XML SpringerLink

A new process of extracting vanadium from stone coal

  • 通讯作者:

    Shi-qi Li    E-mail: lishiqi@ustb.edu.cn

  • A new process of extracting vanadium from the stone coal vanadium ore in Fangshankou, Dunhuang area of Gansu Province, China was introduced. Various leaching experiments were carried out, and the results show that the vanadium ore in Fangshankou is difficult to process due to its high consumption of acid and the high leaching rate of impurities. However, the leaching rate can be up to 80% and the content of V2O5 in the residue can be between 0.22%–0.25% in the process of ore fine grinding→oxidation roasting→mixing and ripening→aqueous leaching→P2O4 solvent extraction→sulfuric acid stripping→oxidation and precipitation→decomposition by heat. Also, the quality of flaky V2O5 produced by this process can meet the requirements of GB3283–87. The total leaching rate of vanadium is 70%. Also, three types of wastes are easy to treat. The vanadium extraction process is better in relation to the aspect of environmental protection than the sodium method.
  • A new process of extracting vanadium from stone coal

    + Author Affiliations
    • A new process of extracting vanadium from the stone coal vanadium ore in Fangshankou, Dunhuang area of Gansu Province, China was introduced. Various leaching experiments were carried out, and the results show that the vanadium ore in Fangshankou is difficult to process due to its high consumption of acid and the high leaching rate of impurities. However, the leaching rate can be up to 80% and the content of V2O5 in the residue can be between 0.22%–0.25% in the process of ore fine grinding→oxidation roasting→mixing and ripening→aqueous leaching→P2O4 solvent extraction→sulfuric acid stripping→oxidation and precipitation→decomposition by heat. Also, the quality of flaky V2O5 produced by this process can meet the requirements of GB3283–87. The total leaching rate of vanadium is 70%. Also, three types of wastes are easy to treat. The vanadium extraction process is better in relation to the aspect of environmental protection than the sodium method.