留言板

尊敬的读者、作者、审稿人, 关于本刊的投稿、审稿、编辑和出版的任何问题, 您可以本页添加留言。我们将尽快给您答复。谢谢您的支持!

姓名
邮箱
手机号码
标题
留言内容
验证码
Volume 19 Issue 1
Jan.  2012
数据统计

分享

计量
  • 文章访问数:  246
  • HTML全文浏览量:  53
  • PDF下载量:  9
  • 被引次数: 0
Xiao-bin Li, Hua Ding, Zheng-you Tang, and Ji-cheng He, Formation of internal cracks during soft reduction in rectangular bloom continuous casting, Int. J. Miner. Metall. Mater., 19(2012), No. 1, pp. 21-29. https://doi.org/10.1007/s12613-012-0510-9
Cite this article as:
Xiao-bin Li, Hua Ding, Zheng-you Tang, and Ji-cheng He, Formation of internal cracks during soft reduction in rectangular bloom continuous casting, Int. J. Miner. Metall. Mater., 19(2012), No. 1, pp. 21-29. https://doi.org/10.1007/s12613-012-0510-9
引用本文 PDF XML SpringerLink

Formation of internal cracks during soft reduction in rectangular bloom continuous casting

  • 通讯作者:

    Xiao-bin Li    E-mail: lxb2001230@126.com

  • To investigate the formation of internal cracks in GCr15 bearing steels during the soft reduction process in rectangular bloom continuous casting, fully coupled thermomechanical finite element models were developed using the commercial software MSC.MARC, and microstructures and fractographs were also observed. With the finite element models, the contours of temperature, equivalent plastic strain, and equivalent von Mises stress were simulated. It is observed that the fracture surfaces of internal cracks are covered by cleavage or quasi-cleavage facets. The region of internal cracks in the intergranular brittle fracture mode is in the mushy zone between the zero ductility temperature (ZDT) and the zero strength temperature (ZST). The simulated equivalent plastic strain in the crack region is 2.34%-2.45%, which is larger than the critical strain (0.4%-1.5%), and the equivalent von Mises stress is 1.84-5.05 MPa, which is within the range of critical stress (3.9-7.2 MPa), thus resulting in the occurrence of internal cracks. Reducing the soft reduction amount from 3 to 2 mm can lower the stress under the critical value.
  • Formation of internal cracks during soft reduction in rectangular bloom continuous casting

    + Author Affiliations
    • To investigate the formation of internal cracks in GCr15 bearing steels during the soft reduction process in rectangular bloom continuous casting, fully coupled thermomechanical finite element models were developed using the commercial software MSC.MARC, and microstructures and fractographs were also observed. With the finite element models, the contours of temperature, equivalent plastic strain, and equivalent von Mises stress were simulated. It is observed that the fracture surfaces of internal cracks are covered by cleavage or quasi-cleavage facets. The region of internal cracks in the intergranular brittle fracture mode is in the mushy zone between the zero ductility temperature (ZDT) and the zero strength temperature (ZST). The simulated equivalent plastic strain in the crack region is 2.34%-2.45%, which is larger than the critical strain (0.4%-1.5%), and the equivalent von Mises stress is 1.84-5.05 MPa, which is within the range of critical stress (3.9-7.2 MPa), thus resulting in the occurrence of internal cracks. Reducing the soft reduction amount from 3 to 2 mm can lower the stress under the critical value.