Xiu-mei Guo, Shu-mao Wang, Xiao-peng Liu, Zhi-nian Li, Jian-hua Ye, Hui-ping Yuan, and Li-jun Jiang, Structural characteristics and mechanism of hydrogen-induced disproportionation of the ZrCo alloy, Int. J. Miner. Metall. Mater., 19(2012), No. 11, pp. 1010-1015. https://doi.org/10.1007/s12613-012-0662-7
Cite this article as:
Xiu-mei Guo, Shu-mao Wang, Xiao-peng Liu, Zhi-nian Li, Jian-hua Ye, Hui-ping Yuan, and Li-jun Jiang, Structural characteristics and mechanism of hydrogen-induced disproportionation of the ZrCo alloy, Int. J. Miner. Metall. Mater., 19(2012), No. 11, pp. 1010-1015. https://doi.org/10.1007/s12613-012-0662-7
引用本文 PDF XML SpringerLink

Structural characteristics and mechanism of hydrogen-induced disproportionation of the ZrCo alloy

  • 通讯作者:

    Xiu-mei Guo    E-mail: xiumei418@163.com

  • The intermetallic compound ZrCo was prepared, and its hydrogen-induced disproportionation in hydrogen desorption processes was investigated. The hydrogenation-dehydrogenation thermodynamics of the ZrCo alloy was evaluated by pressure-composition isotherm measurements at different temperatures. The kinetic processes of hydrogen-induced disproportionation at different temperatures under certain pressures were detailedly studied. The disproportionation rate of the ZrCo alloy increased with the increases of temperature and initial hydrogen pressure under experimental conditions. However, the maximum attainable extent of disproportionation did not change much with an increase in temperature or initial hydrogen pressure. The crystallographic structure analysis of the ZrCo alloy combining with its corresponding dehydrogenation kinetic curves under the conditions of an initial hydrogen pressure of 0.2 MPa and a temperature of 723 K indicated that the basic process of disproportionation reactions was composed of four stages:rapid dehydrogenation of ZrCoH3, equilibrium of dehydrogenation, simultaneity of dehydrogenation and disproportionation, and completion of disproportionation.
  • Structural characteristics and mechanism of hydrogen-induced disproportionation of the ZrCo alloy

    + Author Affiliations
    • The intermetallic compound ZrCo was prepared, and its hydrogen-induced disproportionation in hydrogen desorption processes was investigated. The hydrogenation-dehydrogenation thermodynamics of the ZrCo alloy was evaluated by pressure-composition isotherm measurements at different temperatures. The kinetic processes of hydrogen-induced disproportionation at different temperatures under certain pressures were detailedly studied. The disproportionation rate of the ZrCo alloy increased with the increases of temperature and initial hydrogen pressure under experimental conditions. However, the maximum attainable extent of disproportionation did not change much with an increase in temperature or initial hydrogen pressure. The crystallographic structure analysis of the ZrCo alloy combining with its corresponding dehydrogenation kinetic curves under the conditions of an initial hydrogen pressure of 0.2 MPa and a temperature of 723 K indicated that the basic process of disproportionation reactions was composed of four stages:rapid dehydrogenation of ZrCoH3, equilibrium of dehydrogenation, simultaneity of dehydrogenation and disproportionation, and completion of disproportionation.