留言板

尊敬的读者、作者、审稿人, 关于本刊的投稿、审稿、编辑和出版的任何问题, 您可以本页添加留言。我们将尽快给您答复。谢谢您的支持!

姓名
邮箱
手机号码
标题
留言内容
验证码
Volume 20 Issue 5
May  2013
数据统计

分享

计量
  • 文章访问数:  268
  • HTML全文浏览量:  67
  • PDF下载量:  17
  • 被引次数: 0
Khamphee Jitchaiyaphum, Theerawat Sinsiri, Chai Jaturapitakkul, and Prinya Chindaprasirt, Cellular lightweight concrete containing high-calcium fly ash and natural zeolite, Int. J. Miner. Metall. Mater., 20(2013), No. 5, pp. 462-471. https://doi.org/10.1007/s12613-013-0752-1
Cite this article as:
Khamphee Jitchaiyaphum, Theerawat Sinsiri, Chai Jaturapitakkul, and Prinya Chindaprasirt, Cellular lightweight concrete containing high-calcium fly ash and natural zeolite, Int. J. Miner. Metall. Mater., 20(2013), No. 5, pp. 462-471. https://doi.org/10.1007/s12613-013-0752-1
引用本文 PDF XML SpringerLink

Cellular lightweight concrete containing high-calcium fly ash and natural zeolite

  • 通讯作者:

    Theerawat Sinsiri    E-mail: sinsiri@sut.ac.th

  • Cellular lightweight concrete (CLC) with the controlled density of approximately 800 kg/m3 was made from a preformed foam, Type-I Portland cement (OPC), fly ash (FA), or natural zeolite (NZ), and its compressive strength, setting time, water absorption, and microstructure of were tested. High-calcium FA and NZ with the median particle sizes of 14.52 and 7.72 μm, respectively, were used to partially replace OPC at 0, 10wt%, 20wt%, and 30wt% of the binder (OPC and pozzolan admixture). A water-to-binder mass ratio (W/B) of 0.5 was used for all mixes. The testing results indicated that CLC containing 10wt% NZ had the highest compressive strength. The replacement of OPC with NZ decreased the total porosity and air void size but increased the capillary porosity of the CLC. The incorporation of a suitable amount of NZ decreased the setting time, total porosity, and pore size of the paste compared with the findings with the same amount of FA. The total porosity and cumulative pore volume decreased, whereas the gel and capillary pores increased as a result of adding both pozzolans at all replacement levels. The water absorption increased as the capillary porosity increased; this effect depended on the volume of air entrained and the type or amount of pozzolan.
  • Cellular lightweight concrete containing high-calcium fly ash and natural zeolite

    + Author Affiliations
    • Cellular lightweight concrete (CLC) with the controlled density of approximately 800 kg/m3 was made from a preformed foam, Type-I Portland cement (OPC), fly ash (FA), or natural zeolite (NZ), and its compressive strength, setting time, water absorption, and microstructure of were tested. High-calcium FA and NZ with the median particle sizes of 14.52 and 7.72 μm, respectively, were used to partially replace OPC at 0, 10wt%, 20wt%, and 30wt% of the binder (OPC and pozzolan admixture). A water-to-binder mass ratio (W/B) of 0.5 was used for all mixes. The testing results indicated that CLC containing 10wt% NZ had the highest compressive strength. The replacement of OPC with NZ decreased the total porosity and air void size but increased the capillary porosity of the CLC. The incorporation of a suitable amount of NZ decreased the setting time, total porosity, and pore size of the paste compared with the findings with the same amount of FA. The total porosity and cumulative pore volume decreased, whereas the gel and capillary pores increased as a result of adding both pozzolans at all replacement levels. The water absorption increased as the capillary porosity increased; this effect depended on the volume of air entrained and the type or amount of pozzolan.