留言板

尊敬的读者、作者、审稿人, 关于本刊的投稿、审稿、编辑和出版的任何问题, 您可以本页添加留言。我们将尽快给您答复。谢谢您的支持!

姓名
邮箱
手机号码
标题
留言内容
验证码
Volume 21 Issue 9
Sep.  2014
数据统计

分享

计量
  • 文章访问数:  309
  • HTML全文浏览量:  78
  • PDF下载量:  8
  • 被引次数: 0
Xiao-feng Xue, Ze-hua Wang, Ze-hua Zhou, Shao-qun Jiang, Jiang-bo Cheng, Chang-hao Wang,  and Jia Shao, Bonding characteristics of the Al2O3-metal composite coating fabricated onto carbon steel by combustion synthesis, Int. J. Miner. Metall. Mater., 21(2014), No. 9, pp. 886-893. https://doi.org/10.1007/s12613-014-0985-7
Cite this article as:
Xiao-feng Xue, Ze-hua Wang, Ze-hua Zhou, Shao-qun Jiang, Jiang-bo Cheng, Chang-hao Wang,  and Jia Shao, Bonding characteristics of the Al2O3-metal composite coating fabricated onto carbon steel by combustion synthesis, Int. J. Miner. Metall. Mater., 21(2014), No. 9, pp. 886-893. https://doi.org/10.1007/s12613-014-0985-7
引用本文 PDF XML SpringerLink

Bonding characteristics of the Al2O3-metal composite coating fabricated onto carbon steel by combustion synthesis

  • 通讯作者:

    Ze-hua Wang    E-mail: zhwang@hhu.edu.cn

  • The fabrication of an alumina-metal composite coating onto a carbon steel substrate by using a self-propagating high-temperature synthesis technique was demonstrated. The effects of the type and thickness of the pre-coated layer on the binding structure and surface quality of the coating were systematically investigated. The macrostructure, phase composition, and bonding interface between the coating and the substrate were investigated by scanning electronic microscopy (SEM), X-ray diffraction (XRD), and energy-dispersive X-ray spectrometry (EDS). The diffraction patterns indicated that the coating essentially consisted of α-Al2O3, Fe(Cr), and FeO·Al2O3. With an increase in the thickness of the pre-coated working layer, the coating became more smooth and compact. The transition layer played an important role in enhancing the binding between the coating and the substrate. When the pre-coated working layer was 10 mm and the pre-coated transition layer was 1 mm, a compact structure and metallurgical bonding with the substrate were obtained. Thermal shock test results indicated that the ceramic coating exhibited good thermal shock resistance when the sample was rapidly quenched from 800°C to room temperature by plunging into water.
  • Bonding characteristics of the Al2O3-metal composite coating fabricated onto carbon steel by combustion synthesis

    + Author Affiliations
    • The fabrication of an alumina-metal composite coating onto a carbon steel substrate by using a self-propagating high-temperature synthesis technique was demonstrated. The effects of the type and thickness of the pre-coated layer on the binding structure and surface quality of the coating were systematically investigated. The macrostructure, phase composition, and bonding interface between the coating and the substrate were investigated by scanning electronic microscopy (SEM), X-ray diffraction (XRD), and energy-dispersive X-ray spectrometry (EDS). The diffraction patterns indicated that the coating essentially consisted of α-Al2O3, Fe(Cr), and FeO·Al2O3. With an increase in the thickness of the pre-coated working layer, the coating became more smooth and compact. The transition layer played an important role in enhancing the binding between the coating and the substrate. When the pre-coated working layer was 10 mm and the pre-coated transition layer was 1 mm, a compact structure and metallurgical bonding with the substrate were obtained. Thermal shock test results indicated that the ceramic coating exhibited good thermal shock resistance when the sample was rapidly quenched from 800°C to room temperature by plunging into water.