留言板

尊敬的读者、作者、审稿人, 关于本刊的投稿、审稿、编辑和出版的任何问题, 您可以本页添加留言。我们将尽快给您答复。谢谢您的支持!

姓名
邮箱
手机号码
标题
留言内容
验证码
Volume 22 Issue 11
Nov.  2015
数据统计

分享

计量
  • 文章访问数:  184
  • HTML全文浏览量:  36
  • PDF下载量:  11
  • 被引次数: 0
Yuan-ke Mo, Zhi-hao Zhang, Jian-xin Xie, Hua-dong Fu, and Hong-jiang Pan, Improved cold rolling workability of warm rolled Fe-6.5wt%Si electrical steel with columnar grains by annealing, Int. J. Miner. Metall. Mater., 22(2015), No. 11, pp. 1171-1182. https://doi.org/10.1007/s12613-015-1182-z
Cite this article as:
Yuan-ke Mo, Zhi-hao Zhang, Jian-xin Xie, Hua-dong Fu, and Hong-jiang Pan, Improved cold rolling workability of warm rolled Fe-6.5wt%Si electrical steel with columnar grains by annealing, Int. J. Miner. Metall. Mater., 22(2015), No. 11, pp. 1171-1182. https://doi.org/10.1007/s12613-015-1182-z
引用本文 PDF XML SpringerLink

Improved cold rolling workability of warm rolled Fe-6.5wt%Si electrical steel with columnar grains by annealing

  • 通讯作者:

    Jian-xin Xie    E-mail: jxxie@mater.ustb.edu.cn

  • The effects of annealing temperature (with the annealing time being constant at 1 h) on the microstructure, ordering, residual stress, mechanical properties, and subsequent cold rolling workability of Fe-6.5wt%Si electrical steel with columnar grains were investigated, where the steel was warm rolled at 500℃ with a reduction of 95%. The results show that recrystallization began to occur in the sample annealed at 575℃ and that full recrystallization occurred in the sample annealed at 625℃. When the annealing temperature was 500℃ or greater, the extent of reordering in the sample was high, which reduced the room-temperature plasticity. However, annealing at temperatures below 300℃ did not significantly reduce the residual tensile stress on the edge of the warm rolled samples. Considering the comprehensive effects of annealing temperature on the recrystallization, reordering, residual stress, and mechanical properties of the warm rolled Fe-6.5wt%Si electrical steel with columnar grains, the appropriate annealing temperature range is 300℃-400℃. Unlike the serious edge cracks that appeared in the sample after direct cold rolling, the annealed samples could be cold rolled to a total reduction of more than 71.4% without the formation of obvious edge cracks, and bright-surface Fe-6.5wt%Si electrical steel strips with a thickness less than 0.1 mm could be fabricated by cold rolling.
  • Improved cold rolling workability of warm rolled Fe-6.5wt%Si electrical steel with columnar grains by annealing

    + Author Affiliations
    • The effects of annealing temperature (with the annealing time being constant at 1 h) on the microstructure, ordering, residual stress, mechanical properties, and subsequent cold rolling workability of Fe-6.5wt%Si electrical steel with columnar grains were investigated, where the steel was warm rolled at 500℃ with a reduction of 95%. The results show that recrystallization began to occur in the sample annealed at 575℃ and that full recrystallization occurred in the sample annealed at 625℃. When the annealing temperature was 500℃ or greater, the extent of reordering in the sample was high, which reduced the room-temperature plasticity. However, annealing at temperatures below 300℃ did not significantly reduce the residual tensile stress on the edge of the warm rolled samples. Considering the comprehensive effects of annealing temperature on the recrystallization, reordering, residual stress, and mechanical properties of the warm rolled Fe-6.5wt%Si electrical steel with columnar grains, the appropriate annealing temperature range is 300℃-400℃. Unlike the serious edge cracks that appeared in the sample after direct cold rolling, the annealed samples could be cold rolled to a total reduction of more than 71.4% without the formation of obvious edge cracks, and bright-surface Fe-6.5wt%Si electrical steel strips with a thickness less than 0.1 mm could be fabricated by cold rolling.
    • loading

    Catalog


    • /

      返回文章
      返回