U. K. N. Din, T. H. T. Aziz, M. M. Salleh, and A. A. Umar, Synthesis of crystalline perovskite-structured SrTiO3 nanoparticles using an alkali hydrothermal process, Int. J. Miner. Metall. Mater., 23(2016), No. 1, pp. 109-115. https://doi.org/10.1007/s12613-016-1217-0
Cite this article as:
U. K. N. Din, T. H. T. Aziz, M. M. Salleh, and A. A. Umar, Synthesis of crystalline perovskite-structured SrTiO3 nanoparticles using an alkali hydrothermal process, Int. J. Miner. Metall. Mater., 23(2016), No. 1, pp. 109-115. https://doi.org/10.1007/s12613-016-1217-0
引用本文 PDF XML SpringerLink

Synthesis of crystalline perovskite-structured SrTiO3 nanoparticles using an alkali hydrothermal process

  • 通讯作者:

    U. K. N. Din    E-mail: ummiump@yahoo.com

    M. M. Salleh    E-mail: mms@ukm.edu.my

  • We report an experimental route for synthesizing perovskite-structured strontium titanate (SrTiO3) nanocubes using an alkali hydrothermal process at low temperatures without further heating. Furthermore, we studied the influence of heating time (at 180℃) on the crystallinity, morphology, and perovskite phase formation of SrTiO3. The SrTiO3 powder, which is formed via nanocube agglomeration, transforms into cubic particles with a particle size of 120–150 nm after 6 h of hydrothermal sintering. The crystallinity and percentage of the perovskite phase in the product increased with heating time. The cubic particles contained 31.24at% anatase TiO2 that originated from the precursor. By varying the weight ratio of anatase TiO2 used to react with the strontium salt precursor, we reduced the anatase-TiO2 content to 18.8at%. However, the average particle size increased when the anatase-TiO2 content decreased.
  • Synthesis of crystalline perovskite-structured SrTiO3 nanoparticles using an alkali hydrothermal process

    + Author Affiliations
    • We report an experimental route for synthesizing perovskite-structured strontium titanate (SrTiO3) nanocubes using an alkali hydrothermal process at low temperatures without further heating. Furthermore, we studied the influence of heating time (at 180℃) on the crystallinity, morphology, and perovskite phase formation of SrTiO3. The SrTiO3 powder, which is formed via nanocube agglomeration, transforms into cubic particles with a particle size of 120–150 nm after 6 h of hydrothermal sintering. The crystallinity and percentage of the perovskite phase in the product increased with heating time. The cubic particles contained 31.24at% anatase TiO2 that originated from the precursor. By varying the weight ratio of anatase TiO2 used to react with the strontium salt precursor, we reduced the anatase-TiO2 content to 18.8at%. However, the average particle size increased when the anatase-TiO2 content decreased.