留言板

尊敬的读者、作者、审稿人, 关于本刊的投稿、审稿、编辑和出版的任何问题, 您可以本页添加留言。我们将尽快给您答复。谢谢您的支持!

姓名
邮箱
手机号码
标题
留言内容
验证码
Volume 23 Issue 8
Aug.  2016
数据统计

分享

计量
  • 文章访问数:  314
  • HTML全文浏览量:  75
  • PDF下载量:  8
  • 被引次数: 0
Yuan-yuan Zhu, Ling-yun Yi, Wei Zhao, De-sheng Chen, Hong-xin Zhao,  and Tao Qi, Leaching of vanadium, sodium, and silicon from molten V-Ti-bearing slag obtained from low-grade vanadium-bearing titanomagnetite, Int. J. Miner. Metall. Mater., 23(2016), No. 8, pp. 898-905. https://doi.org/10.1007/s12613-016-1305-1
Cite this article as:
Yuan-yuan Zhu, Ling-yun Yi, Wei Zhao, De-sheng Chen, Hong-xin Zhao,  and Tao Qi, Leaching of vanadium, sodium, and silicon from molten V-Ti-bearing slag obtained from low-grade vanadium-bearing titanomagnetite, Int. J. Miner. Metall. Mater., 23(2016), No. 8, pp. 898-905. https://doi.org/10.1007/s12613-016-1305-1
引用本文 PDF XML SpringerLink

Leaching of vanadium, sodium, and silicon from molten V-Ti-bearing slag obtained from low-grade vanadium-bearing titanomagnetite

  • 通讯作者:

    De-sheng Chen    E-mail: dshchen@ipe.ac.cn

    Tao Qi    E-mail: tqgreen@ipe.ac.cn

  • The water leaching process of vanadium, sodium, and silicon from molten vanadium-titanium-bearing (V-Ti-bearing) slag obtained from low-grade vanadium-bearing titanomagnetite was investigated systematically. The results show that calcium titanate, sodium aluminosilicate, sodium oxide, silicon dioxide and sodium vanadate are the major components of the molten V-Ti-bearing slag. The experimental results indicate that the liquid-solid (L/S) mass ratio significantly affects the leaching process because of the respective solubilities and diffusion rates of the components. A total of 83.8% of vanadium, 72.8% of sodium, and 16.1% of silicon can be leached out via a triple counter-current leaching process under the optimal conditions of a particle size below 0.074 mm, a temperature of 90°C, a leaching time of 20 min, an L/S mass ratio of 4:1, and a stirring speed of 300 r/min. The kinetics of vanadium leaching is well described by an internal diffusion-controlled model and the apparent activation energy is 11.1 kJ/mol. The leaching mechanism of vanadium was also analyzed.
  • Leaching of vanadium, sodium, and silicon from molten V-Ti-bearing slag obtained from low-grade vanadium-bearing titanomagnetite

    + Author Affiliations
    • The water leaching process of vanadium, sodium, and silicon from molten vanadium-titanium-bearing (V-Ti-bearing) slag obtained from low-grade vanadium-bearing titanomagnetite was investigated systematically. The results show that calcium titanate, sodium aluminosilicate, sodium oxide, silicon dioxide and sodium vanadate are the major components of the molten V-Ti-bearing slag. The experimental results indicate that the liquid-solid (L/S) mass ratio significantly affects the leaching process because of the respective solubilities and diffusion rates of the components. A total of 83.8% of vanadium, 72.8% of sodium, and 16.1% of silicon can be leached out via a triple counter-current leaching process under the optimal conditions of a particle size below 0.074 mm, a temperature of 90°C, a leaching time of 20 min, an L/S mass ratio of 4:1, and a stirring speed of 300 r/min. The kinetics of vanadium leaching is well described by an internal diffusion-controlled model and the apparent activation energy is 11.1 kJ/mol. The leaching mechanism of vanadium was also analyzed.
    • loading

    Catalog


    • /

      返回文章
      返回