Sasaki Takeshi, Kanagawa Ryoji, and Ohtsuka Toshiaki, In situ IR-RAS investigation of corrosion of tin in air containing H2O, NO2 and SO2 at room temperature, J. Univ. Sci. Technol. Beijing, 10(2003), No. 3, pp. 35-38.
Cite this article as:
Sasaki Takeshi, Kanagawa Ryoji, and Ohtsuka Toshiaki, In situ IR-RAS investigation of corrosion of tin in air containing H2O, NO2 and SO2 at room temperature, J. Univ. Sci. Technol. Beijing, 10(2003), No. 3, pp. 35-38.
引用本文 PDF XML SpringerLink
Materials

In situ IR-RAS investigation of corrosion of tin in air containing H2O, NO2 and SO2 at room temperature

  • 通讯作者:

    Sasaki Takeshi    E-mail: sasaki@eng.hokudai.ac.jp

  • In order to obtain a fundamental understanding of the corrosion behavior of tin in atmosphere, in situ IR-RAS (infrared reflection absorption spectroscopy) measurements were performed on tin in humid air containing SO2 and NO2 at room temperature.Time-resolved in situ IR spectra in air of 90% RH (relative humidity) containing 1×10-5-2.2×10-5 SO2 suggested that the tin oxide layers worked as a protective film and no significant corrosion occurred. The conosion products in air of 80%-90% RH containing 1×10-5-2.2×10-5 NO2 were SnO2, SnO, nitrate and hyponitrite. The synergistic effect of SO2 and NO2 on corrosion of tin was not observed in air of 90% RH containing 0.84×10-6 SO2 and 1.8×10-6 NO2.
  • Materials

    In situ IR-RAS investigation of corrosion of tin in air containing H2O, NO2 and SO2 at room temperature

    + Author Affiliations
    • In order to obtain a fundamental understanding of the corrosion behavior of tin in atmosphere, in situ IR-RAS (infrared reflection absorption spectroscopy) measurements were performed on tin in humid air containing SO2 and NO2 at room temperature.Time-resolved in situ IR spectra in air of 90% RH (relative humidity) containing 1×10-5-2.2×10-5 SO2 suggested that the tin oxide layers worked as a protective film and no significant corrosion occurred. The conosion products in air of 80%-90% RH containing 1×10-5-2.2×10-5 NO2 were SnO2, SnO, nitrate and hyponitrite. The synergistic effect of SO2 and NO2 on corrosion of tin was not observed in air of 90% RH containing 0.84×10-6 SO2 and 1.8×10-6 NO2.
    • loading