Guo-fa Sui, Jin-shan Li, Hong-wei Li, Feng Sun, Tie-bang Zhang,  and Heng-zhi Fu, Investigation on the explosive welding mechanism of corrosion-resisting aluminum and stainless steel tubes through finite element simulation and experiments, Int. J. Miner. Metall. Mater., 19(2012), No. 2, pp. 151-158. https://doi.org/10.1007/s12613-012-0531-4
Cite this article as:
Guo-fa Sui, Jin-shan Li, Hong-wei Li, Feng Sun, Tie-bang Zhang,  and Heng-zhi Fu, Investigation on the explosive welding mechanism of corrosion-resisting aluminum and stainless steel tubes through finite element simulation and experiments, Int. J. Miner. Metall. Mater., 19(2012), No. 2, pp. 151-158. https://doi.org/10.1007/s12613-012-0531-4

Investigation on the explosive welding mechanism of corrosion-resisting aluminum and stainless steel tubes through finite element simulation and experiments

+ Author Affiliations
  • Corresponding author:

    Hong-wei Li    E-mail: lihongwei@nwpu.edu.cn

  • Received: 11 January 2011Revised: 17 February 2011Accepted: 24 February 2011
  • To solve the difficulty in the explosive welding of corrosion-resistant aluminum and stainless steel tubes, three technologies were proposed after investigating the forming mechanism through experiments. Then, a 3D finite element model was established for systematic simulations in the parameter determination. The results show that the transition-layer approach, the coaxial initial assembly of tubes with the top-center-point the detonation, and the systematic study by numerical modeling are the key technologies to make the explosive welding of LF6 aluminum alloy and 1Cr18Ni9Ti stainless steel tubes feasible. Numerical simulation shows that radial contraction and slope collision through continuous local plastic deformation are necessary for the good bonding of tubes. Stand-off distances between tubes (D1 and D2) and explosives amount (R) have effect on the plastic deformation, moving velocity, and bonding of tubes. D1 of 1 mm, D2 of 2 mm, and R of 2/3 are suitable for the explosive welding of LF6-L2-1Cr18Ni9Ti three-layer tubes. The plastic strain and moving velocity of the flyer tubes increase with the increase of stand-off distance. More explosives (R>2/3) result in the asymmetrical distribution of plastic strain and non-bonding at the end of detonation on the tubes.
  • loading
  • 加载中

Catalog

    通讯作者: 陈斌, bchen63@163.com
    • 1. 

      沈阳化工大学材料科学与工程学院 沈阳 110142

    1. 本站搜索
    2. 百度学术搜索
    3. 万方数据库搜索
    4. CNKI搜索

    Share Article

    Article Metrics

    Article Views(313) PDF Downloads(8) Cited by()
    Proportional views

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return