留言板

尊敬的读者、作者、审稿人, 关于本刊的投稿、审稿、编辑和出版的任何问题, 您可以本页添加留言。我们将尽快给您答复。谢谢您的支持!

姓名
邮箱
手机号码
标题
留言内容
验证码
Volume 20 Issue 8
Aug.  2013
数据统计

分享

计量
  • 文章访问数:  248
  • HTML全文浏览量:  55
  • PDF下载量:  7
  • 被引次数: 0
Jin-long Liu, Cheng-ming Li, Rui-hua Zhu, Liang-xian Chen, Jing-jing Wang,  and Zhi-hong Feng, Ohmic contact properties of p-type surface conductive layer on H-terminated diamond films prepared by DC arc jet CVD, Int. J. Miner. Metall. Mater., 20(2013), No. 8, pp. 802-807. https://doi.org/10.1007/s12613-013-0799-z
Cite this article as:
Jin-long Liu, Cheng-ming Li, Rui-hua Zhu, Liang-xian Chen, Jing-jing Wang,  and Zhi-hong Feng, Ohmic contact properties of p-type surface conductive layer on H-terminated diamond films prepared by DC arc jet CVD, Int. J. Miner. Metall. Mater., 20(2013), No. 8, pp. 802-807. https://doi.org/10.1007/s12613-013-0799-z
引用本文 PDF XML SpringerLink

Ohmic contact properties of p-type surface conductive layer on H-terminated diamond films prepared by DC arc jet CVD

  • 通讯作者:

    Cheng-ming Li    E-mail: chengmli@mater.ustb.edu.cn

  • With the advantages of high deposition rate and large deposition area, polycrystalline diamond films prepared by direct current (DC) arc jet chemical vapor deposition (CVD) are considered to be one of the most promising materials for high-frequency and high-power electronic devices. In this paper, high-quality self-standing polycrystalline diamond films with the diameter of 100 mm were prepared by DC arc jet CVD, and then, the p-type surface conductive layer with the sheet carrier density of 1011-1013 cm−2 on the H-terminated diamond film was obtained by micro-wave hydrogen plasma treatment for 40 min. Ti/Au and Au films were deposited on the H-terminated diamond surface as the ohmic contact electrode, respectively, afterwards, they were treated by rapid vacuum annealing at different temperatures. The properties of these two types of ohmic contacts were investigated by measuring the specific contact resistance using the transmission line method (TLM). Due to the formation of Ti-related carbide at high temperature, the specific contact resistance of Ti/Au contact gradually decreases to 9.95 × 10−5 Ω·cm2 as the temperature increases to 820℃. However, when the annealing temperature reaches 850℃, the ohmic contact for Ti/Au is degraded significantly due to the strong diffusion and reaction between Ti and Au. As for the as-deposited Au contact, it shows an ohmic contact. After annealing treatment at 550℃, low specific contact resistance was detected for Au contact, which is derived from the enhancement of interdiffusion between Au and diamond films.
  • Ohmic contact properties of p-type surface conductive layer on H-terminated diamond films prepared by DC arc jet CVD

    + Author Affiliations
    • With the advantages of high deposition rate and large deposition area, polycrystalline diamond films prepared by direct current (DC) arc jet chemical vapor deposition (CVD) are considered to be one of the most promising materials for high-frequency and high-power electronic devices. In this paper, high-quality self-standing polycrystalline diamond films with the diameter of 100 mm were prepared by DC arc jet CVD, and then, the p-type surface conductive layer with the sheet carrier density of 1011-1013 cm−2 on the H-terminated diamond film was obtained by micro-wave hydrogen plasma treatment for 40 min. Ti/Au and Au films were deposited on the H-terminated diamond surface as the ohmic contact electrode, respectively, afterwards, they were treated by rapid vacuum annealing at different temperatures. The properties of these two types of ohmic contacts were investigated by measuring the specific contact resistance using the transmission line method (TLM). Due to the formation of Ti-related carbide at high temperature, the specific contact resistance of Ti/Au contact gradually decreases to 9.95 × 10−5 Ω·cm2 as the temperature increases to 820℃. However, when the annealing temperature reaches 850℃, the ohmic contact for Ti/Au is degraded significantly due to the strong diffusion and reaction between Ti and Au. As for the as-deposited Au contact, it shows an ohmic contact. After annealing treatment at 550℃, low specific contact resistance was detected for Au contact, which is derived from the enhancement of interdiffusion between Au and diamond films.
    • loading

    Catalog


    • /

      返回文章
      返回