Dolochar as a reductant in the reduction roasting of iron ore slimes

摘要: The present investigation examines the viability of dolochar, a sponge iron industry waste material, as a reductant in the reduction roasting of iron ore slimes, which are another waste generated by iron ore beneficiation plants. Under statistically determined optimum conditions, which include a temperature of 900℃, a reductant-to-feed mass ratio of 0.35, and a reduction time of 30-45 min, the roasted mass, after being subjected to low-intensity magnetic separation, yielded an iron ore concentrate of approximately 64wt% Fe at a mass recovery of approximately 71% from the feed iron ore slime assaying 56.2wt% Fe. X-ray diffraction analyses indicated that the magnetic products contain magnetite and hematite as the major phases, whereas the nonmagnetic fractions contain quartz and hematite.

 

Dolochar as a reductant in the reduction roasting of iron ore slimes

Abstract: The present investigation examines the viability of dolochar, a sponge iron industry waste material, as a reductant in the reduction roasting of iron ore slimes, which are another waste generated by iron ore beneficiation plants. Under statistically determined optimum conditions, which include a temperature of 900℃, a reductant-to-feed mass ratio of 0.35, and a reduction time of 30-45 min, the roasted mass, after being subjected to low-intensity magnetic separation, yielded an iron ore concentrate of approximately 64wt% Fe at a mass recovery of approximately 71% from the feed iron ore slime assaying 56.2wt% Fe. X-ray diffraction analyses indicated that the magnetic products contain magnetite and hematite as the major phases, whereas the nonmagnetic fractions contain quartz and hematite.

 

/