留言板

尊敬的读者、作者、审稿人, 关于本刊的投稿、审稿、编辑和出版的任何问题, 您可以本页添加留言。我们将尽快给您答复。谢谢您的支持!

姓名
邮箱
手机号码
标题
留言内容
验证码
Volume 16 Issue 5
Oct.  2009
数据统计

分享

计量
  • 文章访问数:  284
  • HTML全文浏览量:  100
  • PDF下载量:  12
  • 被引次数: 0
T. A. Daniel Sagayaraj, S. Suresh, and M. Chandrasekar, Experimental studies on the erosion rate of different heat treated carbon steel economiser tubes of power boilers by fly ash particles, Int. J. Miner. Metall. Mater., 16(2009), No. 5, pp. 534-539. https://doi.org/10.1016/S1674-4799(09)60092-3
Cite this article as:
T. A. Daniel Sagayaraj, S. Suresh, and M. Chandrasekar, Experimental studies on the erosion rate of different heat treated carbon steel economiser tubes of power boilers by fly ash particles, Int. J. Miner. Metall. Mater., 16(2009), No. 5, pp. 534-539. https://doi.org/10.1016/S1674-4799(09)60092-3
引用本文 PDF XML SpringerLink
Materials

Experimental studies on the erosion rate of different heat treated carbon steel economiser tubes of power boilers by fly ash particles

  • 通讯作者:

    S. Suresh    E-mail: ssuresh@nitt.edu

  • The experimental investigations on the effect of the fly ash particle size, velocity, impingement angle, and feed rate were done with an emphasis on the effect of erosion on annealed SA 210 GrA1 (A) and normalized SA 210 GrA1 (N) carbon steel economizer-tube materials. Erosion rates were evaluated with different impingement angles ranging from 15° to 90°, at four different velocities of 32.5, 35, 37.5, and 40 m/s, and at four different feed rates of fly ash particles of 2, 4, 6 and 8 g/min. The erodent used was fly ash particles, sizes ranging from 50-250 μm of irregular shapes. Erosion rate is found to be the maximum at the impingement angle of 30°. Erosion rates of the carbon steel tube in different heat treatment conditions, annealed and normalized, at a constant velocity of 32.5 m/s with different angles were studied. In all cases of feed rates, impingement angles, particle sizes, and velocities of fly ash particles, it has been found that the erosion rate of the annealed tube is less than that of the normalized tube. Empirical correlations for erosion rate relating the velocity, size, feed rate, and impingement angle of the particles and elongation property of the target materials were arrived. Morphologies of the eroded surface were examined by scanning electron microscope (SEM).
  • Materials

    Experimental studies on the erosion rate of different heat treated carbon steel economiser tubes of power boilers by fly ash particles

    + Author Affiliations
    • The experimental investigations on the effect of the fly ash particle size, velocity, impingement angle, and feed rate were done with an emphasis on the effect of erosion on annealed SA 210 GrA1 (A) and normalized SA 210 GrA1 (N) carbon steel economizer-tube materials. Erosion rates were evaluated with different impingement angles ranging from 15° to 90°, at four different velocities of 32.5, 35, 37.5, and 40 m/s, and at four different feed rates of fly ash particles of 2, 4, 6 and 8 g/min. The erodent used was fly ash particles, sizes ranging from 50-250 μm of irregular shapes. Erosion rate is found to be the maximum at the impingement angle of 30°. Erosion rates of the carbon steel tube in different heat treatment conditions, annealed and normalized, at a constant velocity of 32.5 m/s with different angles were studied. In all cases of feed rates, impingement angles, particle sizes, and velocities of fly ash particles, it has been found that the erosion rate of the annealed tube is less than that of the normalized tube. Empirical correlations for erosion rate relating the velocity, size, feed rate, and impingement angle of the particles and elongation property of the target materials were arrived. Morphologies of the eroded surface were examined by scanning electron microscope (SEM).
    • loading

    Catalog


    • /

      返回文章
      返回