留言板

尊敬的读者、作者、审稿人, 关于本刊的投稿、审稿、编辑和出版的任何问题, 您可以本页添加留言。我们将尽快给您答复。谢谢您的支持!

姓名
邮箱
手机号码
标题
留言内容
验证码
Volume 9 Issue 6
Dec.  2002
数据统计

分享

计量
  • 文章访问数:  302
  • HTML全文浏览量:  85
  • PDF下载量:  10
  • 被引次数: 0
Caijun Zhang, Lin Wang, Kaike Cai, Weixia Yuan, Zhixiang Yu,  and Yang Zou, Influence of flow control devices on metallurgical effects in a large-capacity tundish, J. Univ. Sci. Technol. Beijing, 9(2002), No. 6, pp. 412-416.
Cite this article as:
Caijun Zhang, Lin Wang, Kaike Cai, Weixia Yuan, Zhixiang Yu,  and Yang Zou, Influence of flow control devices on metallurgical effects in a large-capacity tundish, J. Univ. Sci. Technol. Beijing, 9(2002), No. 6, pp. 412-416.
引用本文 PDF XML SpringerLink
Metallurgy

Influence of flow control devices on metallurgical effects in a large-capacity tundish

  • 通讯作者:

    Caijun Zhang    E-mail: zhangcaijun@263.net

  • The influence of flow control devices on metallurgical effects in a large-capacity tundish has been studied carefully with elements tracing, sampling and theoretical prospecting. The results from the studies are (1) in the continuous casting of clean steel, bad control of tundish operation may deteriorate the cleanliness of steel; (2) the cleanliness of steel is deteriorated mainly at the unsteady state; (3) large amount of macro inclusions come from the top slag and the refractory of tundish; (4) installing dam and weir can improve the cleanliness of steel and lighten the influence of steel fluctuation; and (5) the result of theoretical calculation suggests that the inclusions larger than the critical size of 92.6 μm can be floated out from the tundish bath completely.
  • Metallurgy

    Influence of flow control devices on metallurgical effects in a large-capacity tundish

    + Author Affiliations
    • The influence of flow control devices on metallurgical effects in a large-capacity tundish has been studied carefully with elements tracing, sampling and theoretical prospecting. The results from the studies are (1) in the continuous casting of clean steel, bad control of tundish operation may deteriorate the cleanliness of steel; (2) the cleanliness of steel is deteriorated mainly at the unsteady state; (3) large amount of macro inclusions come from the top slag and the refractory of tundish; (4) installing dam and weir can improve the cleanliness of steel and lighten the influence of steel fluctuation; and (5) the result of theoretical calculation suggests that the inclusions larger than the critical size of 92.6 μm can be floated out from the tundish bath completely.