留言板

尊敬的读者、作者、审稿人, 关于本刊的投稿、审稿、编辑和出版的任何问题, 您可以本页添加留言。我们将尽快给您答复。谢谢您的支持!

姓名
邮箱
手机号码
标题
留言内容
验证码
Volume 12 Issue 6
Dec.  2005
数据统计

分享

计量
  • 文章访问数:  261
  • HTML全文浏览量:  77
  • PDF下载量:  8
  • 被引次数: 0
Jinghong Sun, Yazheng Liu, and Leyu Zhou, Simulation of annealing process effect on texture evolution of deep-drawing sheet Stl5, J. Univ. Sci. Technol. Beijing, 12(2005), No. 6, pp. 512-516.
Cite this article as:
Jinghong Sun, Yazheng Liu, and Leyu Zhou, Simulation of annealing process effect on texture evolution of deep-drawing sheet Stl5, J. Univ. Sci. Technol. Beijing, 12(2005), No. 6, pp. 512-516.
引用本文 PDF XML SpringerLink
Materials

Simulation of annealing process effect on texture evolution of deep-drawing sheet Stl5

  • 通讯作者:

    Leyu Zhou    E-mail: zhouleyu@sohu.com

  • A two-dimensional cellular automaton method was used to simulate grain growth during the recrystallization annealing of deep-drawing sheet Stl5, taking the simulated result of recrystallization and the experimental result of the annealing texture of deepdrawing sheet St15 as the initial condition and reference. By means of computer simulation, the microstructures and textures of different periods of grain growth were predicted. It is achieved that the grain size, shape and texture become stable after the grain growth at a constant temperature of 700°C for 10 h, and the advantaged texture components {111 }<110> and {111 }<112> are dominant.
  • Materials

    Simulation of annealing process effect on texture evolution of deep-drawing sheet Stl5

    + Author Affiliations
    • A two-dimensional cellular automaton method was used to simulate grain growth during the recrystallization annealing of deep-drawing sheet Stl5, taking the simulated result of recrystallization and the experimental result of the annealing texture of deepdrawing sheet St15 as the initial condition and reference. By means of computer simulation, the microstructures and textures of different periods of grain growth were predicted. It is achieved that the grain size, shape and texture become stable after the grain growth at a constant temperature of 700°C for 10 h, and the advantaged texture components {111 }<110> and {111 }<112> are dominant.
    • loading

    Catalog


    • /

      返回文章
      返回