Jianzhuo Sun, Yu Pan, Yanjun Liu, Fan Kuang, Ranpeng Lu, and Xin Lu, Strength-ductility synergy strategy of Ti6Al4V alloy fabricated by metal injection molding, Int. J. Miner. Metall. Mater.,(2024). https://doi.org/10.1007/s12613-024-3023-4 |
Interstitial oxygen (O) contamination is still a huge obstacle for metal injection molding (MIM) titanium alloys. Herein, we successfully solve this critical problem by regulating the thermal debinding temperature and adding the oxygen scavenger LaB6. The result shows that the surface oxide layer (with the thickness of 13.4±0.5 nm) of Ti6Al4V powder begins to dissolve into Ti matrix within the temperature range of 663-775°C. Reducing the thermal debinding temperature and adding LaB6 powder can collectively prevent O contamination for MIM Ti alloys. Benefit from the decrease of dissolved O content, the slips of mixed and