Kabamba Tshilombo, Determination of inclusions in liquid steel after calcium treatment, Int. J. Miner. Metall. Mater., 17(2010), No. 1, pp. 28-31. https://doi.org/10.1007/s12613-010-0105-2
Cite this article as:
Kabamba Tshilombo, Determination of inclusions in liquid steel after calcium treatment, Int. J. Miner. Metall. Mater., 17(2010), No. 1, pp. 28-31. https://doi.org/10.1007/s12613-010-0105-2

Determination of inclusions in liquid steel after calcium treatment

+ Author Affiliations
  • Corresponding author:

    Kabamba Tshilombo    E-mail: ktshilombo@csir.co.za

  • Received: 17 February 2009Revised: 20 March 2009Accepted: 25 March 2009
  • Nozzle blocking was eliminated by calcium-treated liquid steel through changing the chemical and phase composition of alumina inclusions in aluminium-killed steel. Three different methods were applied to determine the composition of inclusions in liquid steel: total oxygen content samples, sampling spoon samples, and “lollipop” steel samples. The results show that calcium modification of liquid steel influences the inclusion composition varying from 2wt% to 14wt% depending on the method used. The composition of inclusions contains mainly Al2O3-CaO only, or is associated with SiO2 or MgO depending on the initial input. The methods used in this study are indicators of the inclusion composition but can be improved to quantify the inclusion size.
  • loading
  • 加载中

Catalog

    通讯作者: 陈斌, bchen63@163.com
    • 1. 

      沈阳化工大学材料科学与工程学院 沈阳 110142

    1. 本站搜索
    2. 百度学术搜索
    3. 万方数据库搜索
    4. CNKI搜索

    Share Article

    Article Metrics

    Article Views(259) PDF Downloads(20) Cited by()
    Proportional views

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return