Prinya Chindaprasirt, Ubolluk Rattanasak, Pimdao Vongvoradit, and Supichart Jenjirapanya , Thermal treatment and utilization of Al-rich waste in high calcium fly ash geopolymeric materials, Int. J. Miner. Metall. Mater., 19(2012), No. 9, pp.872-878. https://dx.doi.org/10.1007/s12613-012-0641-z
Citation: Prinya Chindaprasirt, Ubolluk Rattanasak, Pimdao Vongvoradit, and Supichart Jenjirapanya , Thermal treatment and utilization of Al-rich waste in high calcium fly ash geopolymeric materials, Int. J. Miner. Metall. Mater., 19(2012), No. 9, pp.872-878. https://dx.doi.org/10.1007/s12613-012-0641-z

Thermal treatment and utilization of Al-rich waste in high calcium fly ash geopolymeric materials

  • The Al-rich waste with aluminium and hydrocarbon as the major contaminant is generated at the wastewater treatment unit of a polymer processing plant. In this research, the heat treatment of this Al-rich waste and its use to adjust the silica/alumina ratio of the high calcium fly ash geopolymer were studied. To recycle the raw Al-rich waste, the waste was dried at 110℃ and calcined at 400 to 1000℃. Mineralogical analyses were conducted using X-ray diffraction (XRD) to study the phase change. The increase in calcination temperature to 600, 800, and 1000℃ resulted in the phase transformation. The more active alumina phase of active θ-Al2O3 was obtained with the increase in calcination temperature. The calcined Al-rich waste was then used as an additive to the fly ash geopolymer by mixing with high calcium fly ash, water glass, 10 M sodium hydroxide (NaOH), and sand. Test results indicated that the calcined Al-rich waste could be used as an aluminium source to adjust the silica/alumina ratio and the strength of geopolymeric materials. The fly ash geopolymer mortar with 2.5wt% of the Al-rich waste calcined at 1000℃ possessed the 7-d compressive strength of 34.2 MPa.
  • loading

Catalog

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return