Mohammad Esmaeeli, Hamed Khosravi,  and Alireza Mirhabibi, Fabrication method and microstructural characteristics of coal-tar-pitch-based 2D carbon/carbon composites, Int. J. Miner. Metall. Mater., 22(2015), No. 2, pp. 210-216. https://doi.org/10.1007/s12613-015-1063-5
Cite this article as:
Mohammad Esmaeeli, Hamed Khosravi,  and Alireza Mirhabibi, Fabrication method and microstructural characteristics of coal-tar-pitch-based 2D carbon/carbon composites, Int. J. Miner. Metall. Mater., 22(2015), No. 2, pp. 210-216. https://doi.org/10.1007/s12613-015-1063-5

Fabrication method and microstructural characteristics of coal-tar-pitch-based 2D carbon/carbon composites

+ Author Affiliations
  • Corresponding author:

    Hamed Khosravi    E-mail: hkhosravi@mail.kntu.ac.ir

  • Received: 12 May 2014Revised: 30 May 2014Accepted: 4 June 2014
  • The lignin-cellulosic texture of wood was used to produce two-dimensional (2D) carbon/carbon (C/C) composites using coal tar pitch. Ash content tests were conducted to select two samples among the different kinds of woods present in Iran, including walnut, white poplar, cherry, willow, buttonwood, apricots, berry, and blue wood. Walnut and white poplar with ash contents of 1.994wt% and 0.351wt%, respectively, were selected. The behavior of these woods during pyrolysis was investigated by differential thermal analysis (DTA) and thermo gravimetric (TG) analysis. The bulk density and open porosity were measured after carbonization and densification. The microstructural characteristics of samples were investigated by scanning electron microscopy (SEM), X-ray diffraction (XRD), and Fourier-transform infrared (FT-IR) spectroscopy. The results indicate that the density of both the walnut and white poplar is increased, and the open porosity is decreased with the increasing number of carbonization cycles. The XRD patterns of the wood charcoal change gradually with increasing pyrolysis temperature, possibly as a result of the ultra-structural changes in the charcoal or the presence of carbonized coal tar pitch in the composite's body.
  • loading
  • 加载中

Catalog

    通讯作者: 陈斌, bchen63@163.com
    • 1. 

      沈阳化工大学材料科学与工程学院 沈阳 110142

    1. 本站搜索
    2. 百度学术搜索
    3. 万方数据库搜索
    4. CNKI搜索

    Share Article

    Article Metrics

    Article Views(313) PDF Downloads(9) Cited by()
    Proportional views

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return