Dong-hui Liu, Jian-liang Zhang, Xun Xue, Guang-wei Wang, Ke-jiang Li,  and Zheng-jian Liu, Infiltration behavior of sintering liquid on nuclei ores during low-titanium ore sintering process, Int. J. Miner. Metall. Mater., 23(2016), No. 6, pp. 618-626. https://doi.org/10.1007/s12613-016-1274-4
Cite this article as:
Dong-hui Liu, Jian-liang Zhang, Xun Xue, Guang-wei Wang, Ke-jiang Li,  and Zheng-jian Liu, Infiltration behavior of sintering liquid on nuclei ores during low-titanium ore sintering process, Int. J. Miner. Metall. Mater., 23(2016), No. 6, pp. 618-626. https://doi.org/10.1007/s12613-016-1274-4

Infiltration behavior of sintering liquid on nuclei ores during low-titanium ore sintering process

+ Author Affiliations
  • Corresponding author:

    Jian-liang Zhang    E-mail: zhang.jianliang@hotmail.com

  • Received: 21 October 2015Revised: 24 November 2015Accepted: 30 November 2015
  • Sinter strength is dependent not only on the self-intensity of the residual rude and bonding phase but also on the bonding degree between them. The infiltration behavior of sintering liquid on nuclei ores influences the bonding degree, which ultimately determines the sinter strength. Infiltration tests were conducted using micro-sinter equipment. The infiltration area index of original liquid (IAO), infiltration volume index of secondary liquid (IVS), and sinter body bonding strength (SBS) were proposed to study the melt infiltration behavior. The results show that the IVS first increases and then decreases with increasing TiO2 content in adhering fines, whereas the IAO exhibits the opposite behavior. Compared with the original liquid, the secondary liquid shows lower porosity, smaller pores, and more uniform distribution. The SBS increases first and then decreases with increasing IAO and TiO2 content, and reaches a maximum when the IAO and TiO2 contents are approximately 0.5 and 2.0wt%, respectively. The SBS first increases and then tends to be stable with increasing IVS. The TiO2 content is suggested to be controlled to approximately 2.0wt% in low-titanium ore sintering.
  • loading
  • 加载中

Catalog

    通讯作者: 陈斌, bchen63@163.com
    • 1. 

      沈阳化工大学材料科学与工程学院 沈阳 110142

    1. 本站搜索
    2. 百度学术搜索
    3. 万方数据库搜索
    4. CNKI搜索

    Share Article

    Article Metrics

    Article Views(237) PDF Downloads(10) Cited by()
    Proportional views

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return