Cite this article as: |
Li Feng, Chang Guan, Ji-rong Chang, Hai-min Zhai, Guo-sheng An, and Wen-sheng Li, Preparation and performance of a cold gas dynamic sprayed high-aluminum bronze coating, Int. J. Miner. Metall. Mater., 25(2018), No. 11, pp. 1354-1361. https://doi.org/10.1007/s12613-018-1689-1 |
Wen-sheng Li E-mail: Liws@lut.edu.cn
[1] |
H. Koivuluoto, M. Hononkanen, and P. Vuoristo, Cold-sprayed copper and tantalum coatings-Detailed FE-SEM and TEM analysis, Surf. Coat. Technol., 204(2010), No. 15, p. 2353.
|
[2] |
H. Koivuluoto, A. Coleman, K. Murray, M. Kearns, and P. Vuoristo, High pressure cold sprayed (HPCS) and low pressure cold sprayed (LPCS) coatings prepared from OFHC Cu feedstock:Overview from powder characteristics to coating properties, J. Therm. Spray Technol., 21(2012), No. 5, p. 1065.
|
[3] |
V.K. Champagne, The repair of magnesium rotorcraft components by cold spray, J. Fail. Anal. Prev., 8(2008), No. 2, p. 164.
|
[4] |
H. Assadi, T. Schmidt, H. Richter, J.O. Kliemann, K. Binder, F. Gärtner, T. Klassen, and H. Kreye, On parameter selection in cold spraying, J. Therm. Spray Technol., 20(2011), No. 6, p. 1161.
|
[5] |
T. Han, B.A. Gillispie, and Z.B. Zhao, An investigation on powder injection in the high-pressure cold spray process, J. Therm. Spray Technol., 18(2009), No. 3, p. 320.
|
[6] |
Z.C. Shi, X.Y. Zhang, H. Chen, F.Z. Ding, B. Yu, Z.H. Tang, and F. Lu, Properties of cold spray Al/Zn coatings on high-strength steel, J. Mater. Eng., 43(2015), No. 2, p. 14.
|
[7] |
Y. Dai, B. Ma, J. Chen, G. Liu, and L. Cui, Tribological properties of cold sprayed 420 stainless steel coating on magnesium alloy, Ordnance Mater. Sci. Eng., 40(2017), No. 2, p. 118.
|
[8] |
X.L. Zhou, X.K. Wu, H.H. Guo, J.G. Wang, and J.S. Zhang, Deposition behavior of multi-particle impact in cold spraying process, Int. J. Miner. Metall. Mater., 17(2010), No. 5, p. 635.
|
[9] |
W.S. Li, Z.P. Wang, Y. Lu, Y. Gao, and J.L. Xu, Preparation mechanical properties and wear behaviors of novel aluminum bronze for dies, Trans. Nonferrous Met. Soc. China, 16(2006), No. 3, p. 607.
|
[10] |
Y. Lu, H. Zhang, Y.X. Su, W.S. Li, K. Lu, and S.C. Zhang, Effect of iron on as-cast high aluminium bronze's microstructure and properties, Foundry, 56(2007), No. 2, p. 199.
|
[11] |
W.S. Li, Z.P. Wang, Y.K. Lu, Y.H. Jin, L.H. Yuan, and F. Wang, Mechanical and tribological properties of a novel aluminum bronze material for drawing dies, Wear, 261(2006), No. 2, p. 155.
|
[12] |
W.S. Li, Z.P. Wang, Y. Lu, and L.H. Yuan, Corrosion wear behavior of Al-bronzes in 3.5% NaCl solution, J. Mater. Eng. Perform., 15(2006), p. 102.
|
[13] |
W.S. Li, M.N. Zhang, L. He, X.T. Yang, and X.J. Wu, Novel antifriction and wear-resistant composite coating with self-sensing detection and its luminescent properties, Trans. China Weld. Inst., 37(2016), No. 4, p. 73.
|
[14] |
Y.Y. He, W.S. Li, X.T. Yang, L. He, and D.F. Wang, Microstructure and wear behaviors of plasma spray welded high Al bronze coatings on different substrates, Tribology, 34(2014), No. 5, p. 489.
|
[15] |
Y. Lu, X.W. Yang, X.T. Yang, R.Z. Xiao, and P.C. Wang, Research of anti-friction performance of Ni60 alloy coating optimized by multiple high aluminum bronze, J. Funct. Mater., 47(2016), No. 1, p. 1097.
|
[16] |
L.C. Du, W.S. Li, L. He, X.T. Yang, Y. Lv, F.Q. Wang, G.S. An, and L. Feng, Luminescence and wear properties of cold sprayed Cu-14Al-X/phosphorescence composite coating, Surf. Technol., 44(2015), No. 8, p. 31.
|
[17] |
J.G. Pan, Z.S. Fan, D.B. Sun, H.Y. Yu, H.Q. Li, X.D. Wang, and H.M. Meng, Present state and perspectives of roller repaired technology, New Technol. New Process, 2005, No. 3, p. 60.
|
[18] |
Z.P. Wang, Y. Lu, W.S. L, Y.X. Su, X.M. Niu, G.Q. Tian, J.L. Xu, C.S. Zhu, R.Z. Xiao, and L. Feng, Multi-Element Aluminium Bronze Powder and its Preparation Method, Chinese Patent, Appl. 200910021904.1, 2009.
|
[19] |
W.Y. Li and C.J. Li, Characteristic of cold spray, Chin. Surf. Eng., 15(2002), No. 1, p. 12.
|
[20] |
W.Y. Li, C.J. Li, Y.Y. Wang, and G.J. Yang, Effect of parameter of cold sprayed Cu particles on its impacting behavior, Acta Metall. Sin., 41(2005), No. 3, p. 282.
|
[21] |
V.K. Champagne, The Cold Spray Materials Deposition Process:Fundamentals and Applications, Woodhead Publishing Ltd., Cambridge, 2007, p. 164.
|
[22] |
C. Borchers, F. Gärtner, T. Stoltenhoff, and H. Kreye, Microstructural bonding features of cold sprayed face centered cubic metals, J. Appl. Phys., 96(2004), No. 8, p. 4288.
|
[23] |
J.M. Shockley, S. Descartes, P. Vo, E. Irissou, and R.R. Chromik, The influence of Al2O3 particle morphology on the coating formation and dry sliding wear behavior of cold sprayed Al-Al2O3 composites, Surf. Coat. Technol., 270(2015), p. 324.
|
[24] |
Q. Wang and M.X. Zhang, Review on recent research and development of cold spray technologies, Key Eng. Mater., 533(2013), p. 1.
|
[25] |
H. Assadi, H. Kreye, F. Gärtner, and T. Klassen, Cold spraying-a materials perspective, Acta Mater., 116(2016), p. 382.
|