Di-feng Wu, Shu-sen Cheng,  and Zi-jian Cheng, Characteristics of shell thickness in a slab continuous casting mold, Int. J. Miner. Metall. Mater., 16(2009), No. 1, pp. 25-31. https://doi.org/10.1016/S1674-4799(09)60005-4
Cite this article as:
Di-feng Wu, Shu-sen Cheng,  and Zi-jian Cheng, Characteristics of shell thickness in a slab continuous casting mold, Int. J. Miner. Metall. Mater., 16(2009), No. 1, pp. 25-31. https://doi.org/10.1016/S1674-4799(09)60005-4
Metallurgy

Characteristics of shell thickness in a slab continuous casting mold

+ Author Affiliations
  • The key to reduce shell breakout in the continuous casting process is to control shell thickness in the mold. A numerical simulation on the turbulent flow and heat transfer coupled with solidification in the slab mold using the volume of fluid (VOF) model and the enthalpy-porosity scheme was conducted and the emphasis was put upon the flow effect on the shell thickness profiles in longitudinal and transverse directions. The results show that the jet acts a stronger impingement on the shell of narrow face, which causes a zero-increase of shell thickness in a certain range near the impingement point. The thinnest shell on the slab cross-section locates primarily in the center of the narrow face, and secondly near the comer of the wide face. Nozzle optimization can obviously increase the shell thickness and make it more uniform.
  • loading
  • 加载中

Catalog

    通讯作者: 陈斌, bchen63@163.com
    • 1. 

      沈阳化工大学材料科学与工程学院 沈阳 110142

    1. 本站搜索
    2. 百度学术搜索
    3. 万方数据库搜索
    4. CNKI搜索

    Share Article

    Article Metrics

    Article Views(323) PDF Downloads(14) Cited by()
    Proportional views

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return